Poor Rub or Scuff Resistance

Scuffing is visible at delivery

Refer to inadequate drying section

Ink is improperly formulated

Consult your Sun Chemical representative

Chalking; ink is not binding to stock

Pigment to binder ratio in ink is not compatible with stock.  Consult your Sun Chemical representative