Flexographic

Print page

Fill-In

Problem:

Print impression is excessive.

Solution:

Reset plate pressure to “kiss” impression.

______________________________________________________________________

Problem:

Water-based ink pH is too low.

Solution:

Increase water-based ink pH.

______________________________________________________________________

Problem:

Ink is drying too fast.

Solution:

Add slower drying solvents to reduce tack. Tacky inks will usually show stringing from type edges.

______________________________________________________________________

Problem:

Plates are worn, uneven, cupped or poorly made.

Solution:

Check plates and replace if necessary.

______________________________________________________________________

Problem:

Ink viscosity is too high.

Solution:

Reduce ink viscosity.

______________________________________________________________________

Problem:

Plate relief height is incorrect.

Solution:

Adjust plate relief to correct height range.

______________________________________________________________________

Problem:

Foreign matter appears in ink.

Solution:

Filter or replace ink; eliminate source of contamination.

______________________________________________________________________

Problem:

Ink out of balance – pigment to resin, resin to solvent.

Solution:

Add resin and refresh ink; make sure the correct solvent is being used. Make sure ink is well mixed.

*The solutions provided from the troubleshooting guide are general in nature, please contact your sales or technical representative to discuss specific issues.

flexo-coffee-package-transforms-into-owl

Information about Sun Chemical

Sun Chemical offers a broad portfolio of inks, coatings, color software and brand color management for flexographic printing.

Learn About Sun Chemical's Solutions for Flexographic Printing