Brittleness

Problem:

Web heat is excessive.

Solution:

Decrease web temperature.

______________________________________________________________________

Problem:

Moisture is lost from the substrate.

Solution:

Introduce moisture by adding steam or add a small amount of plasticizer.

______________________________________________________________________

Problem:

The level of plasticizer in the ink is incorrect or plasticizer is lost through migration.

Solution:

Add plasticizer or change ink.

______________________________________________________________________

Problem:

Excessive non-stick is occurring.

Solution:

Reduce non stick or add a small amount of plasticizer.

*The solutions provided from the troubleshooting guide are general in nature, please contact your sales or technical representative to discuss specific issues.

flexo-coffee-package-transforms-into-owl

Information about Sun Chemical

Sun Chemical offers a broad portfolio of inks, coatings, color software and brand color management for gravure printing.

Learn About Sun Chemical's Printing Solutions for Gravure